Corrosion behaviour of Sn-containing oxide layer on AZ91D alloy formed by plasma electrolytic oxidation

期刊

SURFACE & COATINGS TECHNOLOGY
卷 202, 期 17, 页码 4145-4152

出版社

ELSEVIER SCIENCE SA
DOI: 10.1016/j.surfcoat.2008.03.010

关键词

PEO; AZ91D magnesium alloy; anodic film; stannate; corrosion

向作者/读者索取更多资源

Corrosion phenomenon of magnesium alloys is one of the limits for using magnesium alloys in automotive and aerospace industries. The aim of this study is the development of Sn-containing protective oxide coating by a simple plasma electrolytic oxidation in KOH/KF/Na3PO4 electrolyte on AZ91D magnesium alloy in galvanostatic mode. The film morphology and composition were analysed by SEM coupled with EDS, XRD and Raman spectroscopy. In the oxide, tin is mainly incorporated as crystallised MgSn(OH)(6) compound in the layer. The main properties of Sn-containing oxide coating on AZ91D are both keeping the corrosion rate at open-circuit conditions at an acceptable value, and providing a sufficient passivation plateau to reduce the pitting sensibility. The lather characteristic, revealed by pitting tests, addresses the major drawback of magnesium alloys which often undergo important galvanic coupling in service. Consequently, the addition of low stannate concentration in the electrolyte to form Sn-rich anodic oxide on magnesium alloys represents an interesting way to synthesize protective coatings by PEO in a short time of anodization. (C) 2008 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据