The effect of surface chemistry on the glass transition of polycarbonate (PC) inside cylindrical nanopores is studied. Polycarbonate is melt-wetted into nanoporous anodic aluminum oxide (AAO) treated with hydrophobic alkyl- and fluorosilanes of varying length. The curvature observed at the nanowire tips is consistent with a contact angle descriptive of polycarbonate AAO surface interactions. Differential scanning calorimetry (DSC) thermograrns reveal a distinct broadening of the T-g that is related to the motion of polymer chains at the nanopore wall as well as at the core. DSC and thermal gravimetric analysis (TGA) show that polycarbonate infiltrated into a naked AAO template (without silane treatment) degrades upon heating, suggestive of a surface-catalyzed degradation mechanism. It is further shown that silane treatment largely prevents PC thermal degradation.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据