4.6 Article

Temperature dependence of indentation recovery ratios in austenitic and martensitic shape memory alloys

期刊

SMART MATERIALS AND STRUCTURES
卷 22, 期 7, 页码 -

出版社

IOP PUBLISHING LTD
DOI: 10.1088/0964-1726/22/7/077002

关键词

-

资金

  1. UK-India Educational Research Initiative (UKIERI)
  2. Rolls-Royce Plc

向作者/读者索取更多资源

Instrumented microindentation (IM) on two Ni-Ti shape memory alloys (SMAs), where one is austenitic and the other is martensitic at room temperature, were conducted from 40 to 150 degrees C. Results show that the depth and work recovery ratios, eta(d) and eta(w) respectively, are complementary to each other. While eta(d) decreases gradually with temperature for austenite, it drops markedly for the martensite in the martensite-to-austenite transformation regime. These results affirm the utility of IM for characterizing SMAs.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据