Fifteen percent of the total number of ores to be supplied to feldspar flotation facilities is generally comprised of fine particles under 38 mu m in size. Upgrading of these particles by current commercial beneficiation methods poses an environmental threat besides causing economic losses. In this study, an attempt was made to remove gang minerals containing Fe and Ti from a feldspathic slime sample (-38 mu m) using laboratory scale Jameson flotation cell in the presence of both anionic BD-15 and cationic G-TAP collectors. The finely sized ore was successfully upgraded to produce Na-feldspar suitable for ceramics industry. A Na-feldspar concentrate assaying 0.18% Fe2O3 + TiO2 from a slime sample containing 1.06% Fe2O3 + TiO2 at 50% recovery was obtained. (C) 2010 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据