The joining of DC04 steel to 6016-T4 Al alloy is achieved by laser braze welding using a 4047 (Al-12Si) filler wire and a brazing flux. The dissimilar joining is obtained both by welding the parent 6016 alloy to the 4047 filler wire, producing a continuous bonding without apparent macroscopic flaws, and by reactive wetting of the molten Al alloy on the solid steel, resulting in the formation of a thin layer of Fe-Al-Si intermetallic compounds at the steel/bead interface. The linear strength of the assemblies can be as high as 190 N mm 21, with a failure generally located in the reaction layer of the steel/bead interface. Last, the strength of the assemblies is shown to increase linearly with the reaction layer width.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.5
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据