Rapid decomposition of Direct Blue 6 in neutral solution by Fe-B amorphous alloys

期刊

RSC ADVANCES
卷 5, 期 8, 页码 6215-6221

出版社

ROYAL SOC CHEMISTRY
DOI: 10.1039/c4ra10000j

关键词

-

资金

  1. National Science Foundation of China [51271095]

向作者/读者索取更多资源

The development of environmental-friendly materials for the highly-efficient purification of dye-containing wastewater is important and attractive. In this work, Fe-B amorphous alloy ribbons were fabricated and employed to degrade the azo dye, Direct Blue 6. It shows that Fe-B binary amorphous alloys possess low reaction activation energy (25.43 kJ mol(-1)) and much higher degrading efficiency than their crystalline counterparts and the commercial iron powders. Under the same experimental conditions (25 degrees C, initial pH = 7), the surface area normalized reaction rate constant of Fe84B16 amorphous alloy is approximately 1.8 and 89 times as that of its crystalline alloy and the 300 mesh iron powders, respectively. It indicates that the homogeneous amorphous structure is beneficial to the degradation rate of the zero valent iron. It has been found that boron plays an important role in enhancing the degradation rate because it contributes to the formation of an incompact oxide layer at the metal-water interface. Unlike the dense oxide layer formed on the surface of iron powders, this incompact layer would benefit iron atoms' movement and promote the reduction of contaminants. The present results provide a new amorphous zero valent iron material and a new way of designing proper iron-based alloys for waste-water remediation.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据