4.5 Article

Semi-solid die forging of A16061 wrought aluminium alloy with electromagnetic stirring

出版社

PROFESSIONAL ENGINEERING PUBLISHING LTD
DOI: 10.1243/09544054JEM1120

关键词

semi-solid processing; electromagnetic stirring; solid fraction; forming velocity

资金

  1. National Core Research Center (NCRC) programme

向作者/读者索取更多资源

This study demonstrates the forming process of a semi-solid material with a solid fraction of about 45 per cent after the primary alpha-Al particle in the semi-solid material is globularized during solidification by electromagnetically stirring the molten metal poured out into the sleeve. By theological forming experiments incorporating electromagnetic stirring (EMS) using A16061 alloy, the process parameters are optimized to be of 0.3 m/s of forming velocity, 45 MPa of forming pressure, 10 s of stirring time, and 30 A of stirring current to get the best quality. The product exhibited the highest tensile strength of 312.8 MPa and elongation of 4.51 per cent at positions where the pressure was directly applied to the material and overlapping occurred.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.5
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据