期刊
POWDER TECHNOLOGY
卷 254, 期 -, 页码 591-596出版社
ELSEVIER SCIENCE BV
DOI: 10.1016/j.powtec.2014.01.075
关键词
High energy ball milling; Titania-ceria powders; Nanocrystalline powders; Particle size
Titania alone and several titania-ceria blends of powders were milled by high energy ball milling for different periods of time. Phases, crystal size, particle size and morphology were evaluated. The research has demonstrated that milling reduces the mean crystallite size to less than 30 nm for any time whereas powder particles coalesce into coarse agglomerates. At the same time anatase titania transforms to rutile after 3 hour milling, but a thermal treatment at 700 degrees C for 1 h partially recovers the original crystal structure. The behaviour of ceria-titania blends is similar to that of titania alone, but the reversibility of the anatase-rutile transformation does not occur when the quantity of ceria is greater than a critical level which we have set between the composition with Ce/Ce + Ti ratios of 5 and 10 wt.%. (C) 2014 Elsevier B.V. All rights reserved.
作者
我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。
推荐
暂无数据