Magnetite powder and kaolinite derived from waste iron ore tailings for environmental applications

期刊

POWDER TECHNOLOGY
卷 214, 期 3, 页码 513-518

出版社

ELSEVIER SCIENCE SA
DOI: 10.1016/j.powtec.2011.09.017

关键词

Iron ore tailings; Ferric (hydr)oxide; Charcoal; Reduction roasting; Acid insoluble residue; Dye adsorption

向作者/读者索取更多资源

The present study demonstrated a feasible approach of utilizing waste iron ore tailings in synthesis of value added products for environmental applications. The ferric iron recovered from waste iron ore tailings via acid leaching followed by precipitation as ferric (hydr)oxide was used as feed stock to synthesis magnetite powder by its reductive-roasting with charcoal. Physicochemical characterizations revealed the formation of sufficiently pure magnetite powder with ferric (hydr)oxide to charcoal ratio 1:2 and calcined at 1200 degrees C for 4 h. The magnetic powder as such or coated with polyacrylic acid, was found efficient for removal of a model dye, methylene blue from its solution within 2 min. The acid insoluble residue, generated after iron recovery from iron ore tailings, was characterized as kaolinite. The residue with reasonably good surface area (119 m(2) g(-1)) was also found effective for adsorptive removal of dyes including methylene blue and can find large scale applications in wastewater treatment. Moreover the present study provided further inputs for possible alternative uses of waste iron ore tailings to partly reduce its associated disposal problems. (C) 2011 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据