期刊
POWDER TECHNOLOGY
卷 190, 期 1-2, 页码 89-94出版社
ELSEVIER SCIENCE SA
DOI: 10.1016/j.powtec.2008.04.043
关键词
Composite biomaterial; Biodegradable; Polylactic acid; Apatite; Co-grinding; Porosity
This paper presents the results of a study of the production of porous biodegradable composite materials by co-grinding, followed by scaffolding. Dry powders of polylactic acid and nanocrystalline carbonated apatite, analogous to bone mineral were co-ground in a tumbling ball mill in order to disperse the mineral filler within the polymer. Porous scaffolds were then made by hot moulding the mixture of the two components along with a pore-forming agent which was subsequently eliminated by washing. The mechanical resistance of the scaffolds was evaluated in order to determine the best operating conditions to produce implants offering optimised properties for use as bone substitutes. It was shown that 30 wt.% of filler and 70 wt.% of pore-forming agent produce scaffolds which are sufficiently porous and resistant. (C) 2008 Elsevier B.V. All rights reserved.
作者
我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。
推荐
暂无数据