Supercritical carbon dioxide-assisted silanization of multi-walled carbon nanotubes and their effect on the thermo-mechanical properties, of epoxy nanocomposites

期刊

POLYMER
卷 55, 期 16, 页码 4156-4163

出版社

ELSEVIER SCI LTD
DOI: 10.1016/j.polymer.2014.06.020

关键词

Carbon nanotubes; Composites; Supercritical carbon dioxide

向作者/读者索取更多资源

Supercritical carbon dioxide was employed as the solvent for the functionalization of multi-walled carbon nanotubes (MWCNTs) with an epoxy-capped silane. The silanization protocol was found to be a suitable green alternative to traditional routes that rely on organic solvents for grafting nearly monolayers of silane molecules onto the nanotube surfaces. The addition of silanized MWCNTs to a model epoxy markedly increased its T-g, and measurements of the network cooperativity length scale linked this change to a reduction in polymer segment mobility. Composites filled with low loading levels of both pristine and silanized MWCNTs exhibited significantly higher strain at break and toughness than the neat epoxy, and the greatest improvements were observed at low loading levels. SEM analysis of the composite fracture surfaces revealed that nanotube pullout was the primary failure mechanism in epoxy loaded with pristine MWCNTs while crack bridging predominated in composites containing silanized MWCNTs as the result of strong interfacial bonding with the matrix. The elevated Tg and toughness achieved with small additions of silanized MWCNTs promise to extend the engineering applications of the epoxy resin. (C) 2014 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据