By cold drawing the amorphous PLLA sample at 65 degrees C (just above the glass transition temperature of PLLA), a set of uniaxially oriented samples with various draw ratios was prepared. The mesomorphic ordering and chain orientation in PLLA mesophase induced by the cold drawing process was examined by the WAXD and polarized FTIR techniques. Of note, it is interesting to find that the characteristic backbone vibration mode of PLLA mesophase around 918 cm(-1), which has been firstly identified by Stoclet et al. in previous study [Macromolecules 2010, 7228-7237], actually demonstrates a symmetrical peak shifting with increasing the draw ratio. By considering the WAXD data, the correlation between the peak positions for this characteristic backbone vibration mode (located around 918-921 cm(-1)) that related to the chain conformation and the distance of interchain packing in PLLA mesophase obtained at various draw ratios was revealed. (c) 2012 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据