The phase relations of Fe-6.4 wt% Si and Fe-9.9 wt% Si have been investigated up to 130 GPa and 2,600 K based on in situ synchrotron X-ray diffraction measurements in a laser-heated diamond-anvil cell along with chemical analysis of the quenched samples using a field-emission electron probe microanalyzer. We found that the maximum solubility of silicon in solid hcp-iron increases with increasing pressure. Linear extrapolation of the phase boundary between hcp + B2 and hcp phases for Fe-9.9 wt% Si suggests that the solid hcp-iron can include more than 9.9 wt% Si at the Earth's inner-core conditions. If silicon is a major light element in the outer core, a substantial amount of silicon may be incorporated into the inner core during inner-core solidification.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.2
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据