In studying the dehydration of surface-moistened fumed silica Aerosil powders, we found a conductivity percolation transition at low hydration levels. Both the percolation exponent and the threshold are typical for correlated site-bond transitions in complex two-dimensional (2D) systems. The exponent values, 0.94-1.10, are indicative of severe heterogeneity in the conducting medium. The surface moisture at the percolation threshold takes on a universal value of 0.65 mg([H2O])/m([silica])(2), independent of the silica grain size, and equivalent to twice the first hydration monolayer. This level is just sufficient to sustain a quasi-2D, hydrogen-bonded water network spanning the silica surface.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据