4.4 Article

Influence of carbon-nanotube diameters on composite dielectric properties

期刊

出版社

WILEY-V C H VERLAG GMBH
DOI: 10.1002/pssa.201329254

关键词

chemical vapor deposition; electrical properties; polymer-matrix composites; thermal analysis

资金

  1. European Social Fund under the Global Grant measure (Lithuanian team)
  2. EU [FP7-266529 ByNanoEra, PIRSES-2012-31861750 FAEMCAR]
  3. Belarusian Foundation for Basic research project BRFFI [F12Lat-007, FP7-PEOPLE-2013-IRSES-610875 NAmi-ceMC]
  4. Ministry of education and science of the Russian Federation [8748]

向作者/读者索取更多资源

The dielectric properties of polymethylmetacrylate (PMMA) composites filled with CVD made multiwalled carbon nanotubes (MWCNT) of different mean outer diameters (d similar to 9 nm and 12-14 nm) were investigated in the temperature range from 300 to 420 K and in a wide frequency range (20 Hz to 1 MHz). Below the percolation threshold the temperature dependence of the complex dielectric permittivity of the investigated composites is mainly caused by beta relaxation in pure PMMA matrix and the dielectric permittivity is found to be higher in composites with thicker nanotubes. The activation energy of beta relaxation increases with carbon nanotube concentration. The percolation threshold is lower in composites with both thinner and oxidized carbon nanotubes. The established influence of both the MWCNT mean outer diameter and their oxidation on the broadband dielectric characteristics can be exploited for the production of effective low-cost electromagnetic and/or antistatic coatings working at different temperatures. (C) 2013 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.4
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据