4.5 Article

Dental light-cured nanocomposites based on a dimethacrylate matrix: Thermal degradation and isoconversional kinetic analysis in N2 atmosphere

期刊

THERMOCHIMICA ACTA
卷 599, 期 -, 页码 63-72

出版社

ELSEVIER SCIENCE BV
DOI: 10.1016/j.tca.2014.11.017

关键词

Thermogravimetric analysis (TGA); Dimethacrylate nanocomposites; Isoconversional kinetic analysis; Activation energy

向作者/读者索取更多资源

The thermal degradation of five commercial dental nanocomposites, based on a dimethacrylate matrix, was studied using thermogravimetric analysis in order to retrieve information on the structure of the macromolecular network formed. Grandio, Protofill-nano, Filtek (TM) Supreme XT Body, Tetric (R) EvoCeram and Filtek (TM) Supreme XT Translucent were tested under four different heating rates up to 700 degrees C in an inert (N-2) atmosphere. The data provided thus were sufficient not only for a complete record of the decomposition steps in each case, but also for performing a kinetic analysis based on isoconversional methods. The variation of the activation energy as a function of the extent of degradation was estimated using an integral and a differential method. It resulted that the heating endurance of a composite is mainly a matter of the constituents building its polymeric matrix as well as its relative amount. The nature of the inorganic filler little affects the degradation in overall. From the isoconversional analysis at least two degradation steps were revealed depending on the type and the amount of dimethacrylate monomers used. Defect structures formed in the polymeric network during polymerisation resulted in lower initial activation energy values. (C) 2014 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.5
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据