4.7 Article

Acidic sulphate leaching of chalcopyrite concentrates in presence of pyrite

期刊

MINERALS ENGINEERING
卷 24, 期 5, 页码 381-386

出版社

PERGAMON-ELSEVIER SCIENCE LTD
DOI: 10.1016/j.mineng.2010.11.008

关键词

Copper concentrate; Chalcopyrite; Pyrite; Leaching; Galvanic effect

资金

  1. Swedish Research Council Formas [229-2009-657]

向作者/读者索取更多资源

Copper concentrates with mineralogy dominated by chalcopyrite have slow leaching kinetics at atmospheric pressure in sulphate media because of the formation of passivation layer on its surface during the leaching. To enhance the leaching rate of the copper concentrate, pyrite was added to act as a catalyst. Pyrite and copper sulphide minerals then form a galvanic cell which increases both the copper leaching rate and yield. Effect of parameters such as solution redox potential, temperature, initial acid concentration, solids content, total initial iron concentration and pyrite to copper sulphide minerals mass ratio were investigated. Mineralogical analyses by XRD were performed on selected leach residues and the feed materials. A copper recovery higher than 80% in 24 h was achieved at a redox potential of 410 mV vs Ag, AgCl, a temperature of 85 degrees C, 15 g/L of initial acid concentration, a solid content of 7.8% (w/v), a total initial iron concentration 5 g/L and pyrite to copper sulphide minerals mass ratio 2:1. XRD patterns on leach residues showed that candidates for surface passivation, i.e. jarosite and elemental sulphur, were formed at high total initial iron concentrations. (C) 2010 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据