A two-step process for boron recovery from borax sludge is proposed in the present work. The borax sludge was leached with sulphuric acid solution. Then, for the removal of alkaline species from the leachate, calcium and magnesium were precipitated by adjusting the pH of leachate using 1.5 M NaOH and 1.5 M HCl solutions. The effects of pH, temperature, concentration and time on the precipitation process were investigated. It was determined that the calcium and magnesium concentrations in the leachate were reduced from 121 mg/L to 2.6 mg/L and from 145 mg/L to 4.0 mg/L, respectively, at a pH value of 12, a temperature of 70 degrees C, an initial boron concentration of 500 mg/L and a precipitation time of 3 h. Under these optimum conditions, it was observed that the boron concentration in the solution decreased very slightly. In this process, the alkaline species were successfully separated from the boron. Finally, borax pentahydrate (Na(2)B(4)O(7)-5H(2)O) was produced by the evaporation of the final solution obtained after precipitation process. (C) 2010 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据