High-Temperature Mechanical Behavior of Extruded Mg-Y-Zn Alloy Containing LPSO Phases

出版社

SPRINGER
DOI: 10.1007/s11661-013-1628-8

关键词

-

资金

  1. CSIC
  2. Ministry of Science and Innovation [MAT 2009-07811]

向作者/读者索取更多资源

The high-temperature mechanical behavior of extruded Mg97-3x Y-2x Zn (x) (at. pct) alloys is evaluated from 473 K to 673 K (200 A degrees C to 400 A degrees C). The microstructure of the extruded alloys is characterized by Long Period Stacking Ordered structure (LPSO) elongated particles within the magnesium matrix. At low temperature and high strain rates, their creep behavior shows a high stress exponent (n = 11) and high activation energy. Alloys behave as a metal matrix composite where the magnesium matrix transfers part of its load to the LPSO phase. At high-temperature and/or low stresses, creep is controlled by nonbasal dislocation slip. At intermediate and high strain rates at 673 K (400 A degrees C) and at intermediate strain rates between 623 K and 673 K (350 A degrees C and 400 A degrees C), the extruded alloys show superplastic deformation with elongations to failure higher than 200 pct. Cracking of coarse LPSO second-phase particles and their subsequent distribution in the magnesium matrix take place during superplastic deformation, preventing magnesium grain growth.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据