4.6 Article Proceedings Paper

Identification of Defect Prone Peritectic Steel Grades by Analyzing High-Temperature Phase Transformations

出版社

SPRINGER
DOI: 10.1007/s11661-013-1671-5

关键词

-

资金

  1. Austrian Federal Government (Bundesministerium fur Verkehr, Innovation und Technologie)
  2. Austrian Federal Government (Bundesministerium fur Wirtschaft und Arbeit)
  3. Styrian Provincial Government

向作者/读者索取更多资源

Continuous casting of peritectic steels is often difficult and critical; bad surface quality, cracks, and even breakouts may occur. The initial solidification of peritectic steels within the mold leads to formation of surface depressions and uneven shell growth. As commercial steels are always multicomponent alloys, the influence also of the alloying elements besides carbon on the peritectic phase transition needs to be taken into account. Information on the solidification sequence and phase diagrams for initial solidification are lacking especially for new steel grades, like high-alloyed TRIP-steels with high Mn, Si, and particularly high Al contents. Based on a comprehensive method development, the current study shows that differential scanning calorimeter measurements allow a clear prediction if an alloy is peritectic (i.e., critical to cast). In order to confirm these results, thermo-optical analyses with a high-temperature laser-scanning-confocal-microscope are performed to observe the phase transformations in situ up to the melting point. (C) The Minerals, Metals & Materials Society and ASM International 2013

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据