相关参考文献
注意:仅列出部分参考文献,下载原文获取全部文献信息。Quantification of growth kinetics and adherence of oxide scales formed on Ni-based superalloys at high temperature
E. Fedorova et al.
CORROSION SCIENCE (2010)
Crystallographic fatigue crack initiation in nickel-based superalloy Rene 88DT at elevated temperature
Jiashi Miao et al.
ACTA MATERIALIA (2009)
Determination of crystallographic orientation of dwell-fatigue fracture facets in Ti-6242 alloy
V. Sinha et al.
JOURNAL OF MATERIALS SCIENCE (2007)
Crystallography of fracture facets in a near-alpha titanium alloy
V Sinha et al.
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE (2006)
Observations on the faceted initiation site in the dwell-fatigue tested Ti-6242 alloy: Crystallographic orientation and size effects
V Sinha et al.
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE (2006)
Nickel-based superalloys for advanced turbine engines: Chemistry, microstructure, and properties
TM Pollock et al.
JOURNAL OF PROPULSION AND POWER (2006)
Understanding the contributions of normal-fatigue and static loading to the dwell fatigue in a near-alpha titanium alloy
V Sinha et al.
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE (2004)
Evidence for internal oxidation during oxygen enhanced crack growth in P/M Ni-based superalloys
CF Miller et al.
SCRIPTA MATERIALIA (2003)