4.6 Article Proceedings Paper

Crack Progression during Sustained-Peak Low-Cycle Fatigue in Single-Crystal Ni-Base Superalloy Ren, N5

向作者/读者索取更多资源

Crack progression during compressive sustained-peak low-cycle fatigue (SPLCF) was examined in vapor phase aluminide coated single-crystal Ni-base superalloy Ren, N5. Strain-controlled tests with a 120-second hold at compression were conducted at 1366 K (1093 A degrees C) with A = -1 (R = -a) and 0.35 pct total strain range, and were terminated at selected fractions of predicted life. Crack lengths on the surface and crack depth in longitudinal sections were examined for each specimen. All cracks appeared to have initiated at the coating surface. Failed specimens showed that cracks initially grew on (001), perpendicular to the stress axis, and then deflected to other crystallographic planes. Interrupted test specimens showed crevices initiated on the coating surface at less than 10 pct of the predicted life. The depths of crevices into the coating increased with cyclic exposure, but they did not penetrate into the substrate through the interdiffusion zone (IDZ) until about 80 pct of predicted life. Stress relaxation during compressive hold results in residual tension upon unloading. These results suggest that improving creep resistance of the substrate alloy and developing a coating system that can delay crack penetration into the substrate are keys for improved SPLCF life.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据