We have investigated the age-hardening responses and corresponding microstructures of Mg-0.3Ca-xZn (x = 0.0, 0.1, 0.3, 0.6, 1.0, 1.6 at.%) alloys by hardness test, transmission electron microscopy (TEM), and high-angle annular dark field-scanning transmission electron microscopy (HAADF-STEM). Zn additions up to x = 0.6 lead to enhanced age-hardening responses with the highest peak hardness of HV = 69 for x = 0.6. Further addition of Zn degraded the age-hardening responses. HAADF-STEM images revealed that the finely dispersed monolayer G.P. zones with internal ordered structure are the major contributor to the age-hardening. Excess addition of Zn resulted in the formation of Ca2Mg6Zn3 precipitates suppressing the formation of the ordered G.P. zones. (C) 2009 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据