Spark plasma sintering (SPS) parameters including pressure, temperature, holding time and heating rate were considered and optimized to investigate the sintering process of bulk copper. The relationship between the sintering parameters and the microstructure of the bulk compact were obtained and studied. It was concluded that large-size ultrafine-grained copper with an average grain size less than 2.2 mu m and a relative density greater than 96% could be prepared by the SPS process with initial pressure of 1 MPa, holding pressure of 50 MPa, sintering temperature of 750 degrees C, holding time of 6 min and heating rate of 80 degrees C/min. The production process improved the mechanical properties. (c) 2007 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据