Materials Produced From Plant Biomass. Part II: Evaluation of Crystallinity and Degradation Kinetics of Cellulose

出版社

UNIV FED SAO CARLOS, DEPT ENGENHARIA MATERIALS
DOI: 10.1590/S1516-14392012005000048

关键词

Eucalyptus grandis; Pinus taeda; cellulose; crystallinity; FTIR spectroscopy; thermal degradation

资金

  1. CAPES

向作者/读者索取更多资源

In this study Eucalyptus grandis (CEG) and Pinus taeda (CPT) cellulose fibers obtained from kraft and sulfite pulping process, respectively, were characterized using Fourier transform infrared (FTIR) spectroscopy and thermogravimetry (TGA). The degradation kinetic parameters were determined by TGA using Coats and Redfern method. FTIR results showed that CPT presented a more ordered structure with higher crystallinity than CEG. Thermogravimetric results showed that CPT had a higher thermal stability than CEG. The kinetic results revel that for CEG the degradation mechanism occurs mainly by random nucleation, although phase boundary controlled reactions also occurs while for CPT the degradation process is more related with phase boundary controlled reactions. Results demonstrated that differences between thermal stability and degradation mechanisms might be associated with differences in the cellulose crystalline structure probably caused by different pulping processes used for obtaining the cellulose fibers.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.0
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据