4.6 Article

Direct coating of cubic boron nitride with titanium powder under high pressure and high temperature

期刊

MATERIALS LETTERS
卷 123, 期 -, 页码 210-213

出版社

ELSEVIER SCIENCE BV
DOI: 10.1016/j.matlet.2014.02.107

关键词

Composite materials; Crystal structure; Raman; Cubic boron nitride; Coatings

资金

  1. Natural Science Foundation of China [51203109, 51172089]
  2. SXNSF [2013021008-2]
  3. Qualified Personnel Foundation of Taiyuan University of Technology (QPFT) [tyutrc-201372a]
  4. Youth Foundation of Taiyuan University of Technology [2013Y009, 2013Z072]

向作者/读者索取更多资源

this paper, we propose a facile one-step method for preparing cubic boron nitride (cBN) composite materials. In this method, the pure titanium nitride (TiN) coatings are grown on cBN at 5.0 GPa and 1400-1650 degrees C during a crystal growth process. We investigate the composition and the microstructure of the coatings. The results indicate that the uniformity of TiN coatings formed on cBN surface can be controlled by the temperature and Ti powder content. The average residual stress of TiN-coated cBN is less than 0.64 GPa. We find that the crystal growth process plays an important role in direct coating of cBN. This one-step method of direct coating of cBN is an effective way to facilitate the preparation of coated cBN composite materials. (C) 2014 Elsevier B.V. All rights reserved.