A series of LaNb3O9 Samples was prepared at 1325-1360 degrees C by the solid state reaction. The structures, temperature dependence of thermally stimulated Currents and impedances were investigated. The samples show single phase of LaNb3O9 by XRD analysis. The SEM analysis exhibits that the grain size increases and the porosity factor decreases with increasing sintering temperature. The stimulated current decreases with increasing sintering temperature and a large current of similar to 110 mu A without applied voltage was observed in the LaNb3O9 sample sintered at 1325 degrees C. The polarization-electric field and temperature dependence of impedance results suggest that the temperature dependence Of Current does not originate from pyroelectric effect, but from the release of thermally stimulated current. (C) 2009 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据