Study on hot corrosion reactions between SmYbZr2O7 ceramic and vanadium pentoxide at temperatures of 600-1000°C in air

期刊

MATERIALS CHEMISTRY AND PHYSICS
卷 130, 期 3, 页码 1134-1138

出版社

ELSEVIER SCIENCE SA
DOI: 10.1016/j.matchemphys.2011.08.044

关键词

Ceramics; Corrosion test; Energy dispersive analysis of X-rays; Microstructure

资金

  1. National Natural Science Foundation of China (NSFC) [50972030, 51002038, 51021002]
  2. Fundamental Research Funds for the Central Universities [HIT.BRET1.2010006]

向作者/读者索取更多资源

SmYbZr2O7 ceramic powders were pressureless-sintered at 1700 degrees C for 10 h to fabricate dense bulk materials. SmYbZr2O7 exhibited a single phase of defect fluorite-type structure. Hot corrosion tests between SmYbZr2O7 and V2O5 were carried out in an electric furnace at temperatures of 600-1000 degrees C for 2 h in air, respectively, and the reaction products were investigated using X-ray diffraction, laser Raman spectroscopy and scanning electron microscopy. The final corrosion products were composed of (Sm,Yb)VO4 and ZrV2O7 or m-ZrO2, depending upon the reaction temperature. Hot corrosion mechanisms were further discussed based on the thermal instability of ZrV2O7 at elevated temperatures. (C) 2011 Elsevier B.V. All rights reserved.