Effect of post weld heat treatments on microstructure and mechanical properties of friction stir welded joints of Al-Zn-Mg alloy AA7039

期刊

MATERIALS & DESIGN
卷 43, 期 -, 页码 134-143

出版社

ELSEVIER SCI LTD
DOI: 10.1016/j.matdes.2012.06.018

关键词

Friction stir welding; Post weld heat treatment; Microstructure; Abnormal grain growth; Mechanical properties; Aluminum alloy

资金

  1. DST, Govt. of India [SR/S3/MERC/005/2009]
  2. MHRD, Govt. of India

向作者/读者索取更多资源

Friction stir welded joints of Al-Zn-Mg aluminum alloy AA7039 were given five different post weld heat treatments in order to investigate their effect on microstructure and mechanical properties. In general, all the applied post weld heat treatments increased the size of a aluminum grains in all zones of friction stir weld joints. Abnormal grain growth was observed in entire zone modified by friction stir welding in case of solution treated joints with and without artificial aging. The naturally aged joints offered the highest mechanical properties while solution treated joints offered lowest mechanical properties of the joints. Naturally aged joints yielded highest tensile strength (94.9%) and elongation (174.2%) efficiencies while artificially aged joints yielded highest yield strength efficiency (96.7%). Further, post weld heat treatment also affected fracture location and mode of fracture. (c) 2012 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据