期刊
MACROMOLECULAR MATERIALS AND ENGINEERING
卷 293, 期 7, 页码 631-640出版社
WILEY-BLACKWELL
DOI: 10.1002/mame.200800045
关键词
copper nanowires; electrical conductivity; mixing; nanocomposites; percolation; resistivity
Polystyrene and copper nanowires were melt-mixed at 200 degrees C and 50 rpm in 5 mL and 15 mL DSM co-rotating conical micro-compounders (DSM5 and DSM15), respectively. The electrical, morphological and rheological properties of the resulting nanocomposites were studied. The electrical percolation of nanocomposites is between 1.0 and 2.0 vol.-% for the composites prepared in DSM5 and above 2.0 vol.-% for the composites prepared in DSM15. SEM micrographs show smaller copper nanowire agglomerates inside polystyrene from DSM15 than those from DSM5. However, TEM micrographs reveal that both single copper nanowires and nanowire bundles coexist in the polymer matrix for the samples prepared in both micro-compounders. No obvious microstructure transition is detected by the dynamic rheological data at 200 degrees C.
作者
我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。
推荐
暂无数据