4.7 Article

Structural and thermal behavior of proclay kaolinite using high energy ball milling process

期刊

POWDER TECHNOLOGY
卷 271, 期 -, 页码 228-237

出版社

ELSEVIER SCIENCE BV
DOI: 10.1016/j.powtec.2014.11.018

关键词

Ball milling; Proclay kaolinite; Thermal behavior; Structure

向作者/读者索取更多资源

Planetary ball mill is used to process kaolinite clay powder under a commercial name of proclay kaolinite. Influence of milling time on structure and thermal behavior of proclay kaolinite are presented and discussed. X-ray powder diffraction shows that peak intensities, at kaolinite characteristic positions, decrease gradually and decay after 3 hours of milling. Amorphous structure of kaolinite forms with a nanocrystalline quartz. The mean crystallite size of nanocrystalline quartz is found to decrease from D = 30 +/- 2 nm for unmilled powder to D = 7 +/- 1.5 nm after 9 hours of processing. For the same time shift, thermal analysis shows that specific heat capacity of unmilled powder increases from 0.93 J/g.K to 1.65 J/g.K for milled powder. (C) 2014 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据