4.7 Article

Fabrication of zero-thermal-expansion ZrSiO4/Y2W3O12 sintered body

期刊

JOURNAL OF THE EUROPEAN CERAMIC SOCIETY
卷 29, 期 15, 页码 3129-3134

出版社

ELSEVIER SCI LTD
DOI: 10.1016/j.jeurceramsoc.2009.06.001

关键词

Composites; Thermal expansion; Yttrium tungstate; Zircon; TMA

资金

  1. Tanigawa Thermal Technology Foundation in Japan

向作者/读者索取更多资源

We focused on the linear negative thermal expansion of Y2W3O12 in a wide-temperature range and on the chemical stability of ZrSiO4 in the fabrication of the composite material ZrSiO4/Y2W3O12 with a zero-thermal-expansion. The compact composed of Y2W3O12 and ZrSiO4 had a thermal shrinkage rate smaller than that of Y2W3O12 and higher than that of ZrSiO4. SEM-EDX observation clarified that the ZrSiO4/Y2W3O12 sintered body fabricated at 1400 degrees C for 10 h had a microstructure composed of ZrSiO4 and Y2W3O12 grains, and XRD indicated that only ZrSiO4 and Y2W3O12 phases existed in the sintered body. The relative density of the ZrSiO4/Y2W3O12 sintered body reached 92%, which was larger than that of the ZrSiO4 sintered body because Y2W3O12 grains could be sintered at lower temperatures. The average linear thermal expansion coefficients of the ZrSiO4/Y2W3O12 sintered body were -0.4 x 10(-6) and -0.08 x 10(-6)degrees C-1 in the temperature ranges from 25 to 500 degrees C and from 25 to 1000 degrees C, respectively, which showed an almost zero-thermal-expansion. (C) 2009 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据