4.7 Article

A new approach to improving flame retardancy, smoke suppression and anti-dripping of PET: Via arylene-ether units rearrangement reactions at high temperature

期刊

POLYMER
卷 77, 期 -, 页码 21-31

出版社

ELSEVIER SCI LTD
DOI: 10.1016/j.polymer.2015.09.016

关键词

2,2 '-(4,4 '-(1,4-phenylenebis(oxy))bis(4,1-phenylene))bis(oxy) diethanol; PET copolyester; Arylene-ether units; Anti melt-dripping; Rearrangement; Flame-retardant-element-free

资金

  1. National Natural Science Foundation of China [50933005, 51421061, J1103315]
  2. Program for Changjiang Scholars and Innovative Research Team in University of Ministry of Education of China [IRT1026]

向作者/读者索取更多资源

In order to avoid the serious melt-dripping problems caused by conventional phosphorus flame retardants, a new arylene-ether containing monomer named 2,2'-(4,4'-(1,4-phenylenebis(oxy))bis(4,1-phenylene)) bis(oxy) diethanol (PBPBD) was synthesized and introduced into the PET main-chain via condensation polymerization. With the incorporation of arylene-ether units, the thermal stability and the char residue from combustion of flame-retardant-element-free copolyesters containing PBPBD (BDxPETs) increased dramatically. However, the crystallinity and melting temperature of these copolymers were lower than the same quantities for PET. Thermal degradation kinetic was investigated using the Ozawa-Flynn-Wall method, which illustrated that the apparent activation energy for decomposition of the copolyesters was enhanced with increasing the conversion and the content of PBPBD. Py-GC/MS results showed that the PBBPD structural units undergo rearrangement reactions at high temperature, and ultimately form conjugated heteroaromatic structures, which lead to the formation of stable char residues with unique stick-shaped micro-morphology. Due to these rearrangement reactions, BDxPETs showed an expected flame retardant performance and a reduction in smoke generation during combustion. For example, the LOI value for BD10PET was 28.4, and the total smoke production (TSP) was 10.4 m(2), much smaller than that for PET, 18.8 m(2). Moreover, melt-dripping was restricted. (C) 2015 Elsevier Ltd. All rights reserved.