期刊
JOURNAL OF THE AMERICAN CERAMIC SOCIETY
卷 97, 期 3, 页码 923-928出版社
WILEY
DOI: 10.1111/jace.12737
关键词
-
资金
- Fundamental R&D Program for Technology of World Premier Materials (WPM)
- Ministry of Trade, Industry and Energy, Republic of Korea
A fully dense SiC ceramic with high thermal conductivity was obtained by conventional hot pressing, with 1vol% Y2O3-Sc2O3 additives. The ceramic had a bimodal microstructure consisting of large and small equiaxed SiC grains. Observation with high-resolution transmission electron microscopy (HRTEM) showed two kinds of homophase (SiC/SiC) boundaries, that is crystallized and clean boundaries, and a fully crystallized junction phase. The thermal conductivity of the SiC ceramic was 234W(mK)(-1) at room temperature. The high thermal conductivity was attributed to a clean SiC lattice and good contiguity between SiC grains.
作者
我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。
推荐
暂无数据