Different types of dense stoichiometric and nonstoichiometric magnesium aluminate (MgAl2O4) spinel (MAS) ceramics were prepared following a conventional double-stage firing process using different commercially available alumina and magnesia raw materials. Stoichiometric, magnesia-rich, and alumina-rich spinels were sintered at 1500 degrees-1800 degrees C for 1-2.5 h. The influence of the different processing parameters (average particle size, degree of spinel phase, green density, mass of the powder compact, sintering temperature, holding time at the peak temperature, and starting composition) on the densification behavior of MAS was assessed by measuring the bulk density, apparent porosity, and water absorption capacity, and microstructural observations. Most of the MAS compositions tested exhibited excellent sintering properties.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据