期刊
JOURNAL OF POWER SOURCES
卷 237, 期 -, 页码 5-12出版社
ELSEVIER SCIENCE BV
DOI: 10.1016/j.jpowsour.2013.02.061
关键词
Lithium ion battery; 1-Ethyl-2,3-trimethyleneimidazolium bis(trifluoromethane sulfonyl)imide ([ETMIm][TFSI]); Solid electrolyte interphase (SEI); Impedance spectroscopy
资金
- U.S. Department of Energy's Office of Basic Energy Science, Division of Materials Sciences and Engineering
- U.S. Department of Energy, the Office of Nuclear Physics
- Oak Ridge Associated Universities (ORAU)
A bicyclic imidazolium ionic liquids, 1-ethyl-2,3-trimethyleneimidazolium bis(tri fluoromethane sulfonyl) imide ([ETMIm][TFSI]), and reference imidazolium compounds, 1-ethyl-3-methylimidazolium bis(trifluoromethane sulfonyl)imide ([EMIm][TFSI]) and 1, 2-dimethyl-3-butylimidazolium bis(trifluoromethane sulfonyl)imide ([DMBIm][TFSI]), were synthesized and investigated as solvents for lithium ion batteries. Although the alkylation at the C-2 position of the imidazolium ring does not affect the thermal stability of the ionic liquids, the stereochemical structure of the molecules has shown profound influences on the electrochemical properties of the corresponding ionic liquids. [ETMIm][TFSI] has better reduction stability than both [EMIm][TFSI] and [DMBIm][TFSI], as confirmed by both linear sweep voltammetry (LSV) and theoretical calculation. Also, a relatively stable solid electrolyte interphase (SEI) is formed in [ETMIm][TFSI], suggested by the time dependence of the impedance spectra of the Li parallel to Li cell. Furthermore, the Li parallel to graphite half-cell based on [BTMIm][TFSI] exhibits reversible capacity of 250 mA h g(-1) and 70 mA h g(-1) at 25 degrees C, which increases to 330 mA h g(-1), and 250 mA h g(-1) at 50 degrees C, under the current rate of C/20 and C/10, respectively. For comparison, the half-cell based on [DMBIm][TFSI] exhibits poor capacity retention under the same current rates at both temperatures. Published by Elsevier B.V.
作者
我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。
推荐
暂无数据