4.8 Article

Study of a proton exchange membrane fuel cells catalyst subjected to anodic operating conditions, by synchrotron-based scanning photoelectron microscopy (SPEM) and high lateral-resolution X-ray photoelectron spectroscopy

期刊

JOURNAL OF POWER SOURCES
卷 196, 期 5, 页码 2513-2518

出版社

ELSEVIER SCIENCE BV
DOI: 10.1016/j.jpowsour.2010.11.039

关键词

SPEM; XPS; Electrocatalyst; Degradation; MEA

向作者/读者索取更多资源

In this paper we report an investigation of the degradation of the Pt/C electrocatalyst of an anodic membrane-electrode assembly (MEA) after 1000 h of operation in a laboratory single-cell PEMFC, using synchrotron-based space-resolved photoelectron spectroscopy. This study is complemented by the analysis of a pristine MEA and reference materials, as well as by electrochemical measurements, SEM imaging and energy-dispersive X-ray fluorescence spectroscopy (EDX). Catalyst ageing correlates with a corrugation of morphology, as observed by SEM and scanning photoelectron microscopy (SPEM), corresponding to Pt nanoparticle agglomeration. Moreover - on the basis of high lateral resolution SPEM, X-ray photoelectron spectroscopy (XPS) and EDX analyses, - we found that, after operation. Pt is transported onto the fibres of the gas-diffusion layer (GDL). Space-resolved XPS shows a peak shift of the Pt 4f(7/2) level to higher and lower binding energies with respect to Pt(1 1 1) and pristine Pt black, respectively, corresponding to nanocrystallinity in the first case and agglomeration in the second one. No oxidised Pt was found in any location of the anodically used MEA. (C) 2010 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.8
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据