Direct methane solid oxide fuel cell working by gradual internal steam reforming: Analysis of operation

期刊

JOURNAL OF POWER SOURCES
卷 193, 期 1, 页码 331-337

出版社

ELSEVIER SCIENCE BV
DOI: 10.1016/j.jpowsour.2008.11.122

关键词

SOFC; Internal reforming; Steam reforming; Methane; Energy

向作者/读者索取更多资源

A solid oxide fuel cell was designed to be operated with pure hydrocarbons, without additive or carrier gas, in order to bring technological simplifications, cost reductions and to extend the fuel flexibility limits. The cell was built-up from a conventional cell (LSM/YSZ/Ni-YSZ), to which was added a Ir-CeO(2) catalyst layer at the anode side and an original current collecting system. The cell was first operated with steam in gradual internal reforming (GIR) conditions (R = [H(2)O]/[CH(4)] < 1) With carrier gas at the anode. The optimal operating parameters were determined in terms of flow rates, cell potential, and fuel utilisation. The cell was finally operated with pure dry methane at 900 degrees C at 0.6 V yielding current density of about 0.1 A cm(-2) at max power for 120 h. Small but abrupt deterioration of the performances was observed. but no carbon deposition. Electrical and chemical analysis of this degradation are provided. At total, the fuel cell was operated for more than 200 h in pure dry methane, demonstrating that gradual internal reforming actually occurred efficiently in the anode compartment, which make possible operation without reforming agent such as H(2)O Or CO(2) for other hydrocarbon fuels. (C) 2008 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.8
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据