期刊
JOURNAL OF POROUS MATERIALS
卷 16, 期 4, 页码 481-486出版社
SPRINGER
DOI: 10.1007/s10934-008-9222-y
关键词
Mesoporous silica MCM-41; Wetting stability; pH adjustment; Hydrothermal treatment of as-synthesized MCM-41
Effect of pH in aqueous media used in the hydrothermal treatment of as-synthesized MCM-41 on the structure and the wetting stability of the resulting materials was studied using XRD, TG-DTA and N(2) adsorption. The long-range structural order and the wetting stability of the mesoporous MCM-41 were improved through hydrothermal treatment of as-synthesized sample at around pH 7 without salt addition. The pH adjustment of aqueous media toward neutral is thought to shift the polymerization equilibrium of silica species around external surface of the micelles to a higher degree of condensation, and to reduce the electrostatic repulsion between the silicate-micelle composites. This leads to the further formation of Si-O-Si network within the silica walls of the mesoporous materials, resulting in the enhancement of the structural stability of MCM-41 samples.
作者
我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。
推荐
暂无数据