Electrochemical properties of lithium hexafluoroarsenate in methyl acetate at various temperatures

期刊

JOURNAL OF MOLECULAR LIQUIDS
卷 187, 期 -, 页码 332-336

出版社

ELSEVIER
DOI: 10.1016/j.molliq.2013.08.019

关键词

Lithium hexafluoroarsenate; Methyl acetate; Specific electroconductivity; Activation energy; Electrochemical window

向作者/读者索取更多资源

Electrical conductivities of LiAsF6 in methyl acetate were measured in concentration range of 0.4269-2.2672 mol . kg(-1) at 253.15, 263.15, 273.15, 283.15, 293.15, 303.15, 313.15, and 323.15 K. Data were treated by using the semi-empirical Casteel-Amis equation at high concentrations. The dependence of conductivities on the temperature was described by the Arrhenius relationship. It was shown that activation energies for conductivity linearly increased with the mole fraction of LiAsF6. The variation tendency of the energies of activation for the conductivities of LiAsF6 in the order of aprotic solvents (propylene carbonate, gamma-butyrolactone, methyl acetate, tetrahydrofuran) has been discussed on the basis of the hypothesis that various conduction mechanisms occur at high concentration in the solvents of low permittivity. The anodic and cathodic stabilities of the LiAsF6 in methyl acetate were measured on a Pt electrode, a wide enough electrochemical stability window being observed. (C) 2013 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据