期刊
JOURNAL OF MATERIALS RESEARCH
卷 23, 期 7, 页码 1961-1972出版社
CAMBRIDGE UNIV PRESS
DOI: 10.1557/JMR.2008.0251
关键词
-
The structure evolution and oxidation behavior of ZrB2-SiC composites in air from room temperature to ultrahigh temperature were investigated using furnace testing, arc jet testing, and thermal gravimetric analysis (TGA). The oxide structure changed with the increasing temperature. SiC content has no apparent influence on the evolution of structure during the oxidation of ZrB2-SiC below 1600 degrees C. However, the evolution of structure for ZrB2-SiC above 1800 degrees C was significantly affected by the SiC content. The formation of the SiC depleted layer in the ZrB2-SiC system not only depends on the surrounding conditions of pressure and temperature but also on the structure distribution of the SiC in the ZrB2 matrix. The apparent recrystallization of the ZrO2 occurred above 1800 degrees C. The SiC content should be controlled at similar to 16% in the ZrB2-SiC system for the ultrahigh-temperature application. The mechanisms of the structure evolution during oxidation in air were also analyzed.
作者
我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。
推荐
暂无数据