4.6 Article

Influence of FSSW parameters on fracture mechanisms of 5182 aluminium welds

期刊

JOURNAL OF MATERIALS PROCESSING TECHNOLOGY
卷 210, 期 11, 页码 1429-1435

出版社

ELSEVIER SCIENCE SA
DOI: 10.1016/j.jmatprotec.2010.03.022

关键词

Friction stir spot welding; 5182 Al alloy; Fracture mechanisms; Opening mode; Residual stress

向作者/读者索取更多资源

The influence of the tool rotational speed, the probe plunge depth and the shoulder penetration depth on weld microstructure and on the weld strength have been studied. The shear tests showed that the friction stir spot welds fail by nugget pullout. Three microstructural factors play a determinant role on the weld's strength: the size and location of the stir zone, and the unwelded interface tip slope. With increasing rotational speed, the shear strength increases because of the larger size of the stir zone. By changing the probe plunge depth the location of the stir zone can be controlled in order to maximize the bonded distance between the interface tip and the central hole left by the probe. The shoulder penetration depth must be sufficient to ensure a horizontal interface tip and therefore avoid fracture by the opening mode (model) during shear loading. (C) 2010 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据