Anisotropic powder from sintered NdFeB magnets by the HDDR processing route

期刊

出版社

ELSEVIER SCIENCE BV
DOI: 10.1016/j.jmmm.2011.07.043

关键词

Anisotropic; NdFeB; HDDR; Recycling

资金

  1. technology strategy board
  2. EPSRC, Birmingham

向作者/读者索取更多资源

Sintered NdFeB-based scrap magnets were recovered and processed using the HD and HDDR routes. The effects of varying the HDDR processing temperature were investigated (over the range 835-930 degrees C). The disproportion was carried out with a pressure ramp to a maximum of 1000 mbar hydrogen pressure with a 1 h hold time at each step and the optimum recombination conditions were set at 100 mbar with a 20 min hold time. Anisotropic NdFeB powder was produced in all cases with the best magnetic properties achieved at a processing temperature of 880 degrees C, producing powder with a remanence of 1.10(+/- 0.02) T and an intrinsic coercivity of 800 (+/- 16) kA m(-1) and giving a (BH)(max) of 129(+/- 2.5) kJ m(-3). (C) 2011 Published by Elsevier B.V.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.5
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据