4.7 Article

Effect of fly ash preliminary calcination on the properties of geopolymer

期刊

JOURNAL OF HAZARDOUS MATERIALS
卷 164, 期 2-3, 页码 634-639

出版社

ELSEVIER
DOI: 10.1016/j.jhazmat.2008.08.065

关键词

Fly ash; Calcination; Geopolymer; Mechanical properties

资金

  1. Cooperative Research Centre for Sustainable Resource Processing

向作者/读者索取更多资源

The influence of preliminary calcination of fly ashes on the geopolymerisation process has been studied. Preliminary calcination at 500 and 800,C causes decarbonation of the fly ash while it also leads to a decrease of the amorphous content of the fly ashes from 60 to 57%. Geopolymer prepared using raw fly ash exhibited a compressive strength 55.7(9.2) MPa, while for 500 and 800 degrees C calcined samples it reduced to 54(5.8) and 44.4(5.4)MPa, respectively. The decrease in compressive strength of the geopolymers is discussed in terms of partial surface crystallisation of the fly ash particles. Reactivity of the fly ash also has been correlated with the shrinkage rate and presence of efflorescence on the surface of geopolymers. (c) 2008 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据