Decolorization of an anthraquinone dye, Reactive Brilliant Blue KN-R by hydrogen peroxide was examined using Fe-containing Y and ZSM-5 zeolites as heterogeneous catalysts. Catalysts were prepared by ion-exchange and coprecipitation methods, and calcined at different temperatures. The surface morphologies, crystalline phases, and chemical-state of the catalysts were characterized by scanning electron microscopy, X-ray diffraction and X-ray photoelectron spectroscopy. Influences of reaction conditions, such as dye concentration, catalyst dosage and solution pH, were evaluated and the relations between catalytic capacity and surface microstructures were discussed. The results showed that Fe-containing Y and ZSM-5 zeolites generally exhibited similar or better catalytic efficiency compared with homogeneous Fenton reagent, with Fe-containing ZSM-5 being more efficient. Synthesis method and calcination temperature affected catalytic efficiency and the stability of catalysts. Fe-containing ZSM-5, which was prepared by coprecipitation and calcined at 450 degrees C, displayed the greatest decolorization capacity. Under the conditions of initial pH 2.5, 30.0 mmol/L H2O2 and 4.0 g/L catalyst, 250 mg/L KN-R could be decolorized over 90% within 20 min. (C) 2008 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据