Corrosion Resistance of SOFC and SOEC Glass-Ceramic Seal Materials in High Temperature Steam/Hydrogen

期刊

出版社

ASME
DOI: 10.1115/1.4006794

关键词

-

向作者/读者索取更多资源

There exists concern that glass-ceramic seal materials may not tolerate the high temperature gaseous environment in solid oxide fuel cell (SOFC) and solid oxide electrolysis cell (SOEC) applications, potentially leading to the poisoning of electrodes by silica and ultimate loss of hermeticity. A mechanism for the loss of silicon from glass seals has been proposed by other workers. To address this concern, material samples of proprietary glass-ceramics were exposed to steam/hydrogen atmospheres at 800 degrees C for up to 1000 h. The mass losses of the samples were measured at intervals and their changes in surface chemistry were analyzed using techniques such as X-ray photoelectron spectroscopy and dynamic secondary ion mass spectroscopy. It was shown that the extent of corrosion depends on composition and surface microstructure and that some glass-ceramics are particularly resistant to steam/hydrogen corrosion. [DOI: 10.1115/1.4006794]

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

3.9
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据