Introduction: This study evaluated in vitro the radiopacity, setting time, flow, film thickness, solubility, and dimensional changes of AH Plus sealer pure (Dentsply De Trey Gmbh, Konstanz, Germany) and containing 5% and 10% of calcium hydroxide. Methods: The study was performed according to the requirements of the ISO 6876:2001 standard and the American National Standards Institute/American Dental Association (ANSI/ADA)'s Specification No. 57. The following tests were performed: setting time, flow, film thickness, dimensional stability, radiopacity, and solubility. Data were analyzed statistically by analysis of variance and the Tukey tests with a significance level of 5%. Results: The addition of 5% or 10% calcium hydroxide to AH Plus sealer did not alter significantly the radiopacity or setting time values (p > 0.05). Adding 10% calcium hydroxide reduced the flow compared with pure AH Plus and AH Plus/5% calcium hydroxide. The addition of 5% and 10% calcium hydroxide increased the solubility and expansion of AH Plus. All materials presented expansion valued above those recommended by the ADA. The addition of calcium hydroxide to the sealer resulted in greater film thickness. Conclusions: The addition of 5% calcium hydroxide did not affect most physical properties of AH Plus sealer. (J Endod 2010;36:1048-1051)
作者
我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。
推荐
暂无数据