A reproducible test to characterise the triboelectric charging of powders during their pneumatic transport

期刊

JOURNAL OF ELECTROSTATICS
卷 69, 期 3, 页码 146-156

出版社

ELSEVIER
DOI: 10.1016/j.elstat.2011.03.003

关键词

Powders; Pneumatic transport; Tribocharging; Electrostatic; Characterisation

向作者/读者索取更多资源

Although several investigations had been carried out to explore the triboelectrification of powders, only few data are available on the experimental procedures and set-ups required to obtain reliable data. The present study deals with the development of a pneumatic test to characterise the tribocharging of fine powders. An experimental device was set up allowing on-line monitoring of the charge of both particles and transport pipes. Experiments were carried out using two types of powder (fine sugar and PVC) coupled with two types of pipe materials (Teflon and nylon). Results showed the extreme importance of the control of the relative humidity, the initial charge of particles and the charge dissipation of the walls to obtain pertinent data. Furthermore, the results showed that solids loadings higher than 1 (kg of solids/kg of air) are not proper to achieve reliable measurements. However, at very dilute solids loading (similar to 0.001) the time evolutions of the electrostatic charge and the mass of the powder follow similar trends so that the tribocharging becomes independent of the solids mass flowrate. This allows accurate assessment of the tribocharging of cohesive powders for which a regular flow cannot be guaranteed. (C) 2011 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.3
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据