4.5 Article

Chinese archaeological artefacts: Microstructure and corrosion behaviour of high-leaded bronzes

期刊

JOURNAL OF CULTURAL HERITAGE
卷 15, 期 3, 页码 283-291

出版社

ELSEVIER FRANCE-EDITIONS SCIENTIFIQUES MEDICALES ELSEVIER
DOI: 10.1016/j.culher.2013.07.007

关键词

High-leaded bronze; Lead globules corrosion; Scanning electron microscopy; mu Raman spectroscopy; Pourbaix diagrams

向作者/读者索取更多资源

Metallographic features of ancient bronze artefacts often hide peculiar micro-chemical processes and corrosion behaviours, which are worth to be studied as they can provide conservators and archaeologists with valuable tools and information. It is widely documented that Chinese bronzes were cast and the way to adjust their properties was to change the alloy composition. In particular, addition of lead, which is insoluble in the bronze matrix, results in the formation of inclusions or globules, which undergo oxidation processes leading to their conversion into corrosion products. The mechanisms through which this occurs were still poorly investigated. The present work was conducted to further study the corrosion behaviour of high-leaded bronze, especially focusing on the behaviour of lead globules. To this aim, a collection of Chinese archaeological bronzes, showing intermediate steps of degradation, were selected and investigated. The use of combined microscopy-based, molecular and elemental, analytical techniques allowed the characterization as well as the precise location of corrosion products, thus enabling us to propose a degradation pathway basing on thermodynamic data provided by Pourbaix diagram. The achieved results will be useful for researchers involved in these kinds of studies to better interpret data obtained. (C) 2013 Elsevier Masson SAS. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.5
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据