The effect of lauryl capping group on protein release and degradation of poly(D,L-lactic-co-glycolic acid) particles

期刊

JOURNAL OF CONTROLLED RELEASE
卷 172, 期 2, 页码 436-443

出版社

ELSEVIER SCIENCE BV
DOI: 10.1016/j.jconrel.2013.05.034

关键词

PLGA; Release; Degradation; Bovine serum albumin; Nanoparticles; Microparticles

向作者/读者索取更多资源

The aim of this study was to investigate the effect of a specific and frequently used end group (lauryl alcohol) on the protein release and degradation kinetics of poly(DL-lactic-co-glycolic acid) particles of different sizes. Lauryl-capped PLGA and uncapped PLGA (referred to as PLGA-capped and PLGA-COOH, respectively) particles (0.3, 1 and 20 mu m) were prepared by a double emulsion solvent evaporation technique. Bovine serum albumin (BSA) was used as a model protein for release studies. During degradation (PBS buffer, pH 7.4 at 37 degrees C), a slower dry mass loss was observed for 0.3 mu m particles than for particles of 1 and 20 mu m. It was further shown that PLGA-capped particles showed slower mass loss likely due to its more hydrophobic nature. It was found that the ester bond hydrolysis rate was substantially slower for PLGA-capped particles and that the rate increased with particle size. Particles showed enrichment in lactic acid content (and thus a decrease in glycolic acid content) in time, and interestingly PLGA-capped particles showed also an enrichment of the lauryl alcohol content. No difference was observed in degradation kinetics between BSA loaded and blank particles. Independent of size, PLGA-COOH based particles showed, after a small burst, a sustained and nearly complete release of BSA during 60-80 days. On the other hand, particles based on PLGA-capped showed a much slower release and exhibited incomplete release, accompanied by the presence of an insoluble residue remaining even after 180 days. FTIR analysis of this residue showed that it contained both polymer and protein. Considering the polymer enrichment in lauryl alcohol, the incomplete release observed for PLGA-capped is likely attributed to interactions between the protein and the lauryl end group. In conclusion, since PLGA-COOH, in contrast to the capped derivative, shows complete degradation as well as quantitative release of an entrapped protein, this polymer is preferred for the design of protein formulations. (C) 2013 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.8
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据